Galvanic corrosion is caused by contact between two unlike metals.

Prepare for the General Aandamp;P Test with study guides, flashcards, and multiple-choice questions. Every question includes hints and comprehensive explanations to ensure you are well-prepared. Get ready to succeed!

Multiple Choice

Galvanic corrosion is caused by contact between two unlike metals.

Explanation:
Galvanic corrosion occurs when two different metals are in electrical contact in the presence of an electrolyte. When metals with different electrode potentials meet, electrons flow from the more active metal to the less active metal through the metal connection, while ions move in the electrolyte to complete the circuit. This makes the more anodic metal oxidize and corrode, while the cathodic metal is relatively protected. The electrolyte—often moisture or salt-containing water—enables this transfer; without an electrolyte, mere contact won’t drive significant corrosion. So, the statement is true: contact between two unlike metals is the key initiating factor, with the environment (electrolyte) enabling the reaction. It’s not limited to water or to heating, though moisture and higher temperatures can speed things up.

Galvanic corrosion occurs when two different metals are in electrical contact in the presence of an electrolyte. When metals with different electrode potentials meet, electrons flow from the more active metal to the less active metal through the metal connection, while ions move in the electrolyte to complete the circuit. This makes the more anodic metal oxidize and corrode, while the cathodic metal is relatively protected. The electrolyte—often moisture or salt-containing water—enables this transfer; without an electrolyte, mere contact won’t drive significant corrosion. So, the statement is true: contact between two unlike metals is the key initiating factor, with the environment (electrolyte) enabling the reaction. It’s not limited to water or to heating, though moisture and higher temperatures can speed things up.

Subscribe

Get the latest from Passetra

You can unsubscribe at any time. Read our privacy policy